Surface analysis of catalyst particles in aqueous solutions
Surface analysis of catalyst particles in aqueous solutions
Surface analysis of catalyst particles in aqueous solutions - The results are relevant for the development of efficient photoelectrodes for the production of green hydrogen
Green hydrogen can be produced directly in a photoelectrochemical cell, splitting water with solar energy. However, this requires the development of super-efficient photoelectrodes that need to co ...
Related Keywords
Jan Peter Toennies ,
Manfred Faubel ,
Hebatallah Ali ,
Robert Seidel ,
Stephan Schlemmer ,
Fritz Haber Institute ,
Chemical Research ,
Bernd Winter ,
Fritz Haber ,
Liquid Microjets ,
Metal Oxide Nanoparticle ,
Aqueous Solution Interface Studied ,
Liquid Microjet Photoemission ,
Publication Date ,
Green Hydrogen ,
Hydrogen ,
Hotoelectrodes ,
Photoelectrochemistry ,
Catalysts ,
Metal Oxides ,
Anoparticles ,
Iron Oxide ,
Natase ,
Hematite ,
Photoelectron Spectroscopy ,
Water Splitting ,