"Carbothermal reduction of red mud for iron extraction and sodium remov" by Huaixuan Feng, Xue Feng She et al.
In this work, the technology of carbothermic reduction was used to extract iron and remove sodium from red mud. The effect of various parameters like reduction time, temperature, and basicity on melting separation and de-alkalization was studied. At the optimum reduction temperature of 1,450°C, the basicity of 1.5, and reduction time of 12 min, the metallization rate and sodium removal reach 96.63 and 90.62%, respectively. Melting and separating conditions gradually improve with the temperature increasing from 1,350 to 1,450°C. At high basicity (R = 2), the condition of melting and separatio...